Produktsuche

 

 

POLYLASER GLOSS WHITE / RPAF / KRAFT SP STABILIZED 120A9/RPAF/FGX6415788238127

Download as pdf

Date06.05.2019 SI
ProductPOLYLASER GLOSS WHITE / RPAF / KRAFT SP STABILIZED 120
Sales CodeA9/RPAF/FGX
EAN6415788238127
Product useProduct designed for laser printed gloss finished logistics and industrial variable information label applications. It can be also used in address labelling or other information labelling in SOHO end-uses. This filmic product has excellent tolerance for temperature and humidity fluctuations.
Typical technical values
FacePOLYLASER GLOSS WHITE
ProductWhite, gloss coated heat stabilised polyester film.
Substance72g/m²DIN 53352
Caliper50µmDIN 53370
Elongation MD130.0%DIN 53455
Elongation CD70.0%DIN 53455
Brightness87%ISO 2470/1
Roughness0.7µmISO 8791PPS 10
Opacity88%ISO 2471
Gloss89%Hunter 75°
CIE Whiteness108%ISO 11475
PrintabilitySuitable for laser and common label printing methods like flexography, screen and offset due to the pre-treatment. Special inks designed for non-absorbent materials should be used. Depending on printer used, especially in low humidity conditions, static electricity might occur. To reduce this effect store your media in temperature and humidity controlled conditions. In critical cases manual feed or bypass tray is recommended. Fan the pile of sheets prior printing in order to release accumulated electric charge.
AdhesiveRPAF
TypeGeneral purpose permanent adhesive for A4 and cut-size applications.
CompositionAcrylic, water borne.
Tack min9NFTM 9
BackingKRAFT SPECIAL STABILIZED 120
ProductWhite woodfree kraft backing paper.
Substance120g/m²ISO 536
Caliper112µmISO 534
Tensile strength MD8.0kN/mISO 1924
Tensile strength CD4.0kN/mISO 1924
Performance
Minimum labelling temperature5 °C
Service temperature-20 °C to 100 °C
Shelf lifeFrom date of manufacture: 24 months, under FINAT defined storage conditions (+20-25°C and RH 40-50%). Prolonged storage at higher temperatures and/or humidity levels will shorten the shelf life.
Information
LimitationsLimited adhesion at low temperatures. The highest end-use temperature must be separately checked together with the face material.
DisclaimerThe performance of the product should always be tested in the actual application conditions. Our recommendations are based on our most current knowledge and experience. As our products are used in conditions beyond our control, we cannot assume any liability for damage caused through their use. Users of our products are solely responsible that the product is suitable for its intended application, and have determined such at their sole discretion. Users must comply with any applicable legislation and/or testing requirements for the finished article, and are responsible for bringing their products to market. This publication does not constitute any warranty, express or implied, and is intended only for the recipient and cannot therefore be transferred to any third party. We cannot assume any liability for the use of our products in conjunction with other materials. All our products are sold subject to UPM Raflatac’s general sales conditions, and you should ensure that any existing laws are observed. This publication replaces all previous versions. All information is subject to change without notice.

 Verfügbarkeit der Produkte

ServiceWidth (mm) / Length (m)
Fastmover220/750
Stock1320/0

 Kennen Sie unsere Service-Optionen?

 Komponenten

 ‭(Hidden)‬ News

 ‭(Hidden)‬ Broschüren

 ‭(Hidden)‬ Weiterführendes Material